Development of a new non-destructive method for analysis of the atmospheric corrosion and corrosion protection of copper and copper alloys
schema:about →
<nc183a95666a54f5e85d8e8ecabfc6ba0b4>
|
schema:alternate |
"Copper--Corrosion--Research--European Union countries" |
schema:about →
<nc183a95666a54f5e85d8e8ecabfc6ba0b2>
|
schema:alternate |
"Copper alloys--Corrosion--Research--European Union countries" |
schema:about →
<nc183a95666a54f5e85d8e8ecabfc6ba0b1>
|
schema:alternate |
"Corrosion and anti-corrosives--Research--European Union countries" |
schema:identifier →
<nc183a95666a54f5e85d8e8ecabfc6ba0b5>
|
schema:property |
"NL-AmRIJ" |
| schema:value | "254835" |
schema:about →
<nc183a95666a54f5e85d8e8ecabfc6ba0b3>
|
schema:alternate |
"Patina of metals" |
schema:isPartOf →
Research report / European Commission, Directorate-General Science, Research and Development ;
| schema:name | "Research report / European Commission, Directorate-General Science, Research and Development ;" |